BED Through hardening steels

  • Aerospace

Spécifications

  • EU
    43CrMo4

Typical composition

  • C
    0,43
  • Cr
    1
  • Mo
    0,2

Applications

• Various wear-resistant mechanical parts.
• Ball screws.
• Flattening rolls.

Mechanical properties

• After heat treatment to UTS 880/1050 N/mm2, this steel can be surface hardened by induction treatment.
• After hardening, surface hardness is approximately 700 Vickers.

Mechanical features

  • Heat treatment
    T + Rv 675°C
  • UTS (N/mm²)
    1000
  • A (%)
    19
  • KCU (J/cm²)
    95
  • Solution treated : H
    Annealed : R
  • Thermo-mechanical treatment : TM
    Quenched and tempered : T+RV
  • Sub-zero treatment : F
    Solution treated and aged : T+RV
BED_FR
Download (PDF, 431 KB)