ARMAD Through hardening steels

  • Defense

Spécifications

  • EU
    32CrMoV12-10

Typical composition

  • C
    0,32
  • Cr
    3,1
  • Mo
    1
  • V
    0,3

Applications

• Gun barrels for firearms when a balance between ultimate tensile strength (UTS) and Impact Toughness (KV) at -40°C is above standard used steel grades.
• For any safety mechanical application for which a balance between strength and impact toughness is needed expecially at low temperatures.

Mechanical properties

• Very good ability to cold hammering and button rifling.
• Opportunity to heat treat above 40 HRC, while maintaining a high level of Charpy Impact Toughness at 20°C and -40°C, enhancing firearm performances in operation.

Mechanical features

  • Heat treatment
    T + Rv 570°C
    T + Rv 610°C
  • UTS (N/mm²)
    1500
    1250
  • A (%)
    15
    20
  • KV -60°C (J)
    80
    200
  • Solution treated : H
    Annealed : R
  • Thermo-mechanical treatment : TM
    Quenched and tempered : T+RV
  • Sub-zero treatment : F
    Solution treated and aged : T+RV
brochure ARMAD 2024
Download (PDF, 8 MB)

See also

This site is registered on wpml.org as a development site. Switch to a production site key to remove this banner.